巴斯夫TPU 1190 A 10 000物性表

发表时间:2026-11-10

巴斯夫TPU 1190 A 10 000物性表

eatures
Hydrolysis Resistant
Low Temperature Flexibility
Microbe Resistant
Forms
Pellets
Processing Method
Extrusion
Injection Molding



Injection
Nominal Value
Unit
Drying Temperature
80 to 90
°C
Drying Time
2.0 to 3.0
hr
Suggested Max Moisture
0.020
%
Rear Temperature
185 to 205
°C
Middle Temperature
195 to 225
°C
Front Temperature
205 to 225
°C
Nozzle Temperature
210 to 230
°C
Processing (Melt) Temp
205 to 225
°C
Mold Temperature
15 to 70
°C
Injection Rate
Slow
 
Back Pressure
5.00 to 15.0
MPa